Conventional graphite enables reversible sodium plating and stripping on current collectors in anode-free sodium batteries, stabilizing cycling from 1C to 10C via an ultrathin, robust SEI.
- Why it matters: Anode-free sodium batteries are constrained by poor reversibility of sodium deposition and removal, which limits practical performance and safety under high-rate operation.
- What they did: The work uses graphite’s dynamic interface—driven by ultrafast mixed ion-electron transport, reversible ether solvent cointercalation, and anisotropic flake architecture—to promote edge-dominant nucleation and efficient charge exchange.
- The result: In ampere hour-level pouch cells, the design delivers 92.3% initial Coulombic efficiency and 84.9% capacity retention after 1100 cycles at 3C, with minimal temperature rise at high rates and no thermal runaway during nail penetration.
The findingWhy it mattersWhat they didThe result
AI summary of the abstract · may contain errors · not medical advice · read the paper.