In ferroaluminate clinker–activated low-clinker supersulfated cement, 15 wt% hemihydrate phosphogypsum yields the best strength-normalized performance, reaching 65.54 MPa at 28 d and 81.56 MPa at 270 d.
- Why it matters: Using hemihydrate phosphogypsum as a sulfate source can cut natural gypsum demand, but sulfate release timing must be matched to hydration and pore refinement to avoid strength losses.
- What they did: Cement blends with 5–25 wt% HPG were tested for compressive strength, and 10, 15, and 20 wt% were analyzed via hydration kinetics, pore-solution chemistry, quantitative phase analysis, and microstructure.
- The result: At 10 wt% HPG, early sulfate depletion limited late ettringite formation and pore refinement, while 20 wt% HPG sustained ettringite/C-(A)-S-H yet left more pores >50 nm, reducing strength efficiency; 15 wt% best coupled sulfate supply, hydrates, and pore refinement, with the lowest 28 d energy- and carbon-intensity indices.
The findingWhy it mattersWhat they didThe result
AI summary of the abstract · may contain errors · not medical advice · read the paper.